Skip to content
Welcome to ATM-Magnet
Application Notes

Magnet industry insights, product updates and application notes from ATM-Magnet.

Magnet Selection for EV Traction Motors

Published:2026-09-11    Category:Application Notes    Views:10

Magnet Selection for EV Traction Motors

Magnet selection for an electric vehicle traction motor is not a search for the strongest available grade. It is a search for the grade that keeps producing the required flux over the whole operating envelope — including the worst combination of high rotor temperature and high demagnetizing field the motor will ever see. A grade that delivers more torque on the test bench but demagnetizes during a sustained climb is not a better magnet; it is a failed design.

The practical task is therefore a trade: energy density against coercivity, both balanced against eddy-current heating, coating durability, supply risk and cost.

What Makes Traction Motors Different

An industrial pump motor and an EV traction motor may use the same magnet family, but they stress it in different ways. Four characteristics define the traction case:

  • Extreme torque density. Every millimetre of rotor volume has to produce maximum torque, which pushes design toward the highest practical energy product.
  • A very wide speed range. Field weakening at high speed applies a strong demagnetizing field along the magnet’s easy axis, exactly when the rotor is hottest.
  • A hot rotor. Compact machines with limited cooling paths run magnets well above ambient, and the inner rotor rarely benefits from the cooling applied to the stator.
  • High electrical frequency. Fast switching inverters and high pole counts impose alternating fields on the magnet, generating eddy-current losses inside the magnet itself.

The result is that coercivity class, not energy number, usually decides whether the design is safe. The energy number then decides how much margin is left for cost and weight.

Reading a Grade Designation

A sintered neodymium grade carries two independent pieces of information: the number is the maximum energy product in MGOe, and the suffix letter is the intrinsic coercivity class, which sets the practical maximum operating temperature.

Suffix Minimum intrinsic coercivity Maximum operating temperature Typical traction motor role
M Approx. 14 kOe 100 °C Rarely suitable for traction duty
H Approx. 17 kOe 120 °C Light-duty or well-cooled auxiliary machines
SH Approx. 20 kOe 150 °C Common baseline for traction rotors
UH Approx. 25 kOe 180 °C Severe duty, aggressive field weakening, poor cooling
EH Approx. 30 kOe 200 °C High-temperature or safety-critical applications

Grades Commonly Used in Traction Motors

Grade Br (kGs) (BH)max (MGOe) Hcj (kOe) Max temperature
N48SH Approx. 13.6–14.1 Approx. 45–48 Approx. 20 minimum 150 °C
N45SH Approx. 13.2–13.7 Approx. 43–46 Approx. 20 minimum 150 °C
N42SH Approx. 12.9–13.3 Approx. 40–43 Approx. 20 minimum 150 °C
N45UH Approx. 13.0–13.5 Approx. 42–45 Approx. 25 minimum 180 °C
N40UH Approx. 12.5–12.9 Approx. 38–40 Approx. 25 minimum 180 °C
N38EH Approx. 12.2–12.6 Approx. 36–39 Approx. 30 minimum 200 °C

Values are typical commercial datasheet ranges at 20 °C and vary by supplier and lot. Always specify guaranteed minimums rather than typical figures, and confirm the coercivity class is met across the whole delivery, not on a single sample.

There is a clear pattern in the table: as the coercivity class rises from SH to UH to EH, the attainable energy product falls. That is the core trade in traction motor design, and it explains why designers fight hard to keep a rotor within the SH temperature band if the circuit allows it.

Demagnetization Is the Governing Failure Mode

A traction magnet fails not by cracking or corroding, but by losing magnetization permanently. This happens when the operating point crosses the knee of the demagnetization curve at temperature. Three variables combine to determine whether that happens, and all three must be evaluated together at worst case:

Factor What it does Design response
Rotor temperature Reduces both Br and Hcj, steepening the loss of coercivity Improve cooling, or step up the coercivity class
Demagnetizing field Pushed by field weakening and fault currents Model the worst-case d-axis current, including short-circuit events
Permeance coefficient Sets the load line; thin magnets in open circuits sit closer to the knee Increase magnet thickness or improve the magnetic circuit

In practice the safe design point is set by the least favourable combination: maximum rotor temperature, maximum demagnetizing current and the minimum coercivity permitted by the grade specification. A magnet that passes at nominal coercivity but fails at the lower tolerance limit is a specification problem, not a material problem — which is why guaranteed minimum Hcj is the number worth controlling.

Eddy-Current Losses and Segmentation

Because sintered NdFeB is electrically conductive, the alternating field seen by a rotating magnet induces eddy currents inside it, producing heat directly in the material that is least able to shed it. These losses rise with electrical frequency, so fast-switching inverters, high pole counts and high speed all make the problem worse — and the heat feeds directly back into the demagnetization margin.

Segmentation is the standard countermeasure. Splitting one pole magnet into several electrically isolated pieces interrupts the eddy-current paths; typical rotors use somewhere between four and twelve segments per pole, with thin insulating layers — commonly epoxy at around 30 µm or less — between them. Reported reductions in magnet loss are substantial, in the range of roughly forty to seventy percent compared with a monolithic block, depending on geometry and frequency.

A related development is raising the resistivity of the magnet material itself. Grain boundary diffusion processes that introduce a rare-earth-rich grain boundary phase can produce a substantially higher-resistivity structure alongside their coercivity benefit, suppressing eddy currents without adding separate insulation layers. This is one reason grain boundary diffusion has become central to traction magnet development rather than a niche technique.

Reducing Heavy Rare Earth Content

Higher coercivity classes traditionally required adding dysprosium or terbium to the bulk alloy. Both are scarce, costly and concentrated in supply, and both dilute the magnetic moment — so raising coercivity this way costs energy density as well as money.

Grain boundary diffusion avoids that penalty. Instead of alloying the whole magnet, a dysprosium or terbium source is diffused in so that the heavy rare earth concentrates in the thin grain boundary phase — typically only tens of nanometres thick — where it does its coercivity work. The interior of each grain keeps its dysprosium-free, high-remanence composition. The outcome is a magnet that reaches a UH or EH coercivity class with far less heavy rare earth than a conventional bulk-alloyed grade would need, and with a higher Br for the same coercivity class.

For a traction motor programme this matters in three ways at once: lower material cost, reduced exposure to rare earth price and supply volatility, and better torque density. It is one of the few changes in magnet technology that improves all three simultaneously, which is why nearly every current traction magnet roadmap depends on it.

Coatings for a Hot, Humid Rotor

Neodymium magnets corrode readily because of their high rare-earth content, and heat accelerates the process. In a traction rotor the environment is unusually demanding: elevated temperature, condensation during thermal cycling, possible coolant exposure, and in some designs a high electric field from an 800 V bus.

Coating Strength Limit in traction service
Nickel-copper-nickel Durable, standard, good handling resistance Conductive, so no electrical isolation between segments
Epoxy Electrical insulation plus corrosion protection Must be qualified for the service temperature and cure
Aluminium-based systems Good salt-spray performance at thin film Process control is demanding
Zinc Low cost, sacrificial Thinner film, less suited to severe duty

Coating choice and segmentation strategy are linked. Where segments are used to interrupt eddy currents, the layers between them must be insulating as well as protective, so a conductive nickel-based coating is not sufficient on its own. Where the design relies on a single monolithic magnet, a conventional nickel or epoxy system may be adequate, and the priority shifts to salt-spray and thermal-cycling performance.

Tolerances, Orientation and Shape

Traction rotors almost always use radially oriented arc segments rather than simple blocks, and in that geometry several parameters that are minor for a flat magnet become critical:

  • Orientation angle, because a lobe or pole that is misoriented relative to the rotor axis produces torque ripple and unbalanced forces.
  • Arc radius and angular tolerance, because segments sit in machined pockets and gaps directly affect flux and noise.
  • Thickness tolerance and parallelism, because magnet thickness variation translates into air-gap variation around the rotor.
  • Edge quality and chipping, because brittle sintered neodymium is handled in volume and edge damage becomes a corrosion initiation site.

These requirements are geometry-specific and should be stated on the drawing rather than inherited from a general grade datasheet. Radial orientation in particular is a tooling and pressing decision, not an inspection decision — it cannot be corrected after the fact.

Verification and Qualification

Characteristic How it is verified
Magnetic properties at temperature Demagnetization curves at the maximum service temperature, not only at 20 °C
Irreversible flux loss Flux measurement before and after a defined thermal exposure, referenced to the customer’s load line
Thermal cycling stability Repeated excursions to the temperature limit with flux tracking
Coating performance Salt spray, adhesion and humidity testing against the specified standard
Dimensional and orientation CMM inspection against drawing, including orientation and pole location
Lot traceability Property data traceable to the delivered lot, with automotive-level documentation where required

A Practical Selection Sequence

  1. Establish the maximum rotor temperature at worst-case duty, including fault and overload events, not the steady-state average.
  2. Model the worst-case demagnetizing field, including field weakening at maximum speed and any short-circuit condition.
  3. Determine the minimum permeance coefficient from the actual magnetic circuit, since the same grade behaves differently in a thin open magnet and a thick closed one.
  4. Set the coercivity class from the temperature and field result, then check it at the minimum permitted coercivity, not at typical.
  5. Choose the energy number from the remaining volume and mass budget, accepting that a higher class reduces the attainable energy product.
  6. Assess eddy-current losses at maximum electrical frequency and decide whether segmentation or a high-resistivity material is required.
  7. Select the coating against the actual rotor environment, and confirm it is compatible with the segmentation strategy.
  8. Specify orientation, arc geometry and tolerances on the drawing, and agree the verification plan before tooling is released.
  9. Validate with temperature-dependent curves and a thermal-exposure flux loss test on the production process, not only on a prototype sample.

Common Selection Mistakes

  • Selecting on Br or (BH)max alone, when coercivity class is what determines whether the magnet survives the duty cycle.
  • Using 20 °C properties in the design calculation and treating the temperature derating as a safety factor rather than a design input.
  • Specifying a coercivity class by its typical value, so that magnets at the bottom of the tolerance band are marginal in service.
  • Ignoring magnet eddy-current losses, then finding the rotor runs hotter than the thermal model predicted.
  • Choosing a conductive coating where segments require electrical isolation.
  • Treating heavy rare earth content as purely a cost issue, missing that bulk-alloyed high-coercivity grades also lose energy density.
  • Leaving orientation angle and arc tolerance to a general standard instead of specifying them per drawing.
  • Qualifying on prototype samples that were produced under laboratory conditions rather than on the production line.

About ATM-Magnet

ATM-Magnet supplies sintered neodymium magnets for traction and industrial motor applications across the energy and coercivity range, including the SH, UH and EH classes used in electric vehicle rotors, together with related magnetic materials. Capabilities include grade selection support against the customer’s load line, grain boundary diffusion grades with reduced heavy rare earth content, radially oriented arc segments cut to drawing, segmented magnet assemblies with insulating layers, and coating selection matched to the rotor environment. Lot-level magnetic property documentation and temperature-dependent data are available to support qualification.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top