Skip to content
Welcome to ATM-Magnet
Application Notes

Magnet industry insights, product updates and application notes from ATM-Magnet.

How to Calculate the Pull Force of a Holding Magnet

Published:2026-10-16    Category:Application Notes    Views:1

The pull force of a holding magnet is the force required to separate it perpendicular from a flat ferromagnetic surface, and it is decided by two quantities: the flux density the magnet can drive into that surface, and the area over which that flux is concentrated. The two are linked by a single equation — the magnetic pressure, or Maxwell stress, formula — so the whole calculation reduces to estimating one number, the flux density at the working interface, and multiplying it by the effective pole face area. This guide shows how to make that estimate for disc magnets, pot magnets and steel-backed assemblies, and how air gaps, steel thickness and temperature erode the ideal result.

What Determines the Pull Force of a Holding Magnet?

A holding magnet works because flux crossing an interface between a magnet pole and steel is pulled toward the steel. The force is not created by the magnet alone; it is created by the field in the air or contact layer between the two parts. That is why a magnet that holds 60 N directly on thick mild steel can lose more than half of that force when a single millimetre of air is introduced, and why the same magnet on a thin painted panel behaves completely differently.

Three factors set the force: how much flux the magnet material can produce, how efficiently the surrounding steel circuit concentrates that flux into the pole face, and how large the effective contact area is. Material strength sets the ceiling, the steel circuit decides how much of that ceiling you actually reach, and the area converts flux density into newtons. Changing the magnet grade alone, without changing the circuit or the contact area, rarely moves the result as much as engineers expect.

“Does doubling the magnet diameter double the pull force?” — No. Force scales with pole face area, so doubling the diameter roughly quadruples the theoretical force, but the flux density at the interface falls at the same time because the magnet becomes flatter relative to its width. In practice the gain is real but smaller than four times, and it must be measured or simulated.

The Magnetic Pressure Formula: One Equation, Four Inputs

For a holding magnet in contact with a much thicker steel body, the attractive force is approximated by the magnetic pressure acting over the effective pole face area:

F = (B² × A) / (2 × μ0)

where B is the flux density at the working interface in tesla, A is the effective pole face area in square metres, and μ0 is the permeability of free space, 4π × 10⁻⁷ H/m. The equation shows the most important practical fact about holding magnets: force depends on flux density squared. A 20% increase in B gives a 44% increase in force, while a 20% loss of B costs 36% of the force. Flux density, not magnet size or grade name, is the number that decides the result.

Symbol Quantity Unit How to Obtain It
F Pull force (normal to the surface) N (newton) Calculated, then verified by pull test
B Flux density at the working interface T (tesla), 1 T = 10,000 G Estimated from circuit, measured with a gaussmeter, or FEA
A Effective pole face (contact) area m² (1 cm² = 1 × 10⁻⁴ m²) Geometry; subtract non-magnetic regions
μ0 Permeability of free space H/m Constant, 4π × 10⁻⁷ = 1.2566 × 10⁻⁶

Because B enters the formula squared, it is more useful to think in terms of magnetic pressure — force per unit area — and then multiply by area. The table below converts the interface flux density a designer can actually measure into a holding pressure, so no calculation is needed beyond choosing the area.

Interface Flux Density B Magnetic Pressure Holding Force per cm² Holding Force per cm²
0.2 T 15.9 kPa 1.6 N 0.16 kgf
0.4 T 63.7 kPa 6.4 N 0.65 kgf
0.5 T 99.5 kPa 10.0 N 1.01 kgf
0.6 T 143.2 kPa 14.3 N 1.46 kgf
0.8 T 254.6 kPa 25.5 N 2.60 kgf
1.0 T 397.9 kPa 39.8 N 4.06 kgf

How Do You Estimate the Flux Density at the Working Interface?

B is the only quantity in the formula that cannot be read from a drawing, and it is the one that separates a rough answer from a useful one. For a magnet in direct contact with thick mild steel, B depends on the material’s remanence, the length-to-diameter ratio of the magnet along its magnetization axis, the thickness and permeability of the steel, and how much of the flux returns through the air rather than through the steel.

Two shortcuts are commonly used. The first is to measure it: assemble the magnet on a representative steel sample and read the flux density with a transverse or axial gaussmeter probe on the steel surface next to the contact face. The second is to estimate from the table below and treat the result as a starting point, then confirm with a pull test. For critical designs, finite element analysis is the appropriate tool because it accounts for the returned flux path, saturation and edge effects that no table can capture.

Magnet or Assembly Type Typical Material Br Typical B at Working Interface Notes
NdFeB disc or block on thick mild steel 1.2–1.4 T 0.40–0.70 T Higher value for taller magnets (higher L/D)
NdFeB pot magnet (steel housing) 1.2–1.4 T 0.50–0.80 T at the pot face Housing concentrates flux into the centre pole
SmCo disc on thick mild steel 0.9–1.1 T 0.35–0.60 T Chosen for high-temperature holding duty
Ferrite (ceramic) block on steel 0.38–0.43 T 0.15–0.30 T Large area needed to reach useful force
NdFeB on austenitic stainless (304 / 316) 1.2–1.4 T below 0.05 T Non-magnetic; not a holding surface

“Why is my magnet’s real pull force lower than the datasheet value?” — Because datasheet pull force assumes direct contact, thick mild steel, room temperature and a perfectly aligned pull. Any air gap, thin or stainless steel, offset load or elevated temperature removes part of that ideal figure.

Worked Examples: From Formula to Newtons

The four cases below use the formula with an assumed interface flux density. They are meant to show the size of the answer and the sensitivity to area, not to replace a measurement. Each result is the theoretical pull-off force with the magnet flat on thick mild steel at room temperature.

Magnet Assumed B Effective Area Calculated Force Equivalent Lifted Mass
Ø25 × 10 mm N42 disc 0.55 T 4.91 cm² 59 N ≈ 6.0 kg
Ø20 × 5 mm N42 disc 0.45 T 3.14 cm² 25 N ≈ 2.6 kg
Ø32 mm N42 pot magnet 0.65 T 5.87 cm² (both poles) 99 N ≈ 10.1 kg
40 × 20 × 10 mm N42 block, magnetized through 10 mm 0.50 T 8.00 cm² 80 N ≈ 8.1 kg

How Much Pull Force Does an Air Gap Cost You?

Air gap is the single largest practical loss. Even a fraction of a millimetre — a paint layer, an anodized finish, a piece of tape or a speck of rust — moves the steel out of the high-flux region and reduces force steeply. The loss scales with the gap measured as a proportion of the effective pole dimension, not in absolute millimetres, so a 0.5 mm gap costs a 25 mm magnet far less than it costs a 5 mm one.

Air Gap (as % of Pole Dimension) Retained Pull Force Typical Cause
0% (direct contact) 100% Clean, flat, magnetic steel
≈ 2% 80–90% Thin paint or coating, smooth surface
≈ 5% 65–80% Thick powder coat, adhesive layer
≈ 10% 50–65% Sheet-metal tolerance stack, plating
≈ 20% 30–45% Deliberate mounting offset, spacer
≈ 40% 15–25% Thick gasket or potting between magnet and steel
≥ 100% under 5% Magnet fully out of the steel circuit

“What is the pull force of a 25 mm N42 disc magnet?” — Against thick mild steel in direct contact, typically about 5–7 kg (50–70 N). The value collapses toward a fraction of that as soon as a gap appears between the magnet and the steel.

Why Does the Steel Behind the Magnet Matter So Much?

The steel is not a passive backing plate; it is the return path for the flux. If it is too thin, it saturates and cannot carry the flux away from the pole face, which forces the magnet to work into a higher-reluctance circuit and lowers B. As a rule of thumb, the steel should be at least three times the effective pole dimension thick for the magnet to deliver its full published force. Below that thickness, force falls quickly.

Backing Material and Condition Relative Holding Force Notes
Mild steel, thickness ≥ 3 × pole dimension 100% Reference condition, no saturation
Mild steel, thickness ≈ 1 × pole dimension 60–80% Approaching saturation in the return path
Mild steel sheet, thickness ≈ 0.5 × 40–60% Strongly saturated; force becomes thickness-limited
Galvanised or thin-painted steel 85–95% Coating acts as a small air gap
Hot-rolled steel with heavy mill scale 70–85% Rough scale lifts the magnet off the surface
Grey cast iron 60–85% Varies with graphite form and section
Austenitic stainless steel 304 / 316 under 2% Effectively non-magnetic
Aluminium, brass, copper, polymer 0% No attraction at all

What Else Reduces Pull Force in a Real Assembly?

Within the useful range, the pull force calculator gives the normal, perpendicular force. Real installations rarely load the magnet that way, and several effects stack on top of the air-gap loss.

  • Shear and side load. A magnet that resists 60 N of direct pull may slide under only 15–25 N of sideways force, because shear capacity is limited by friction (typically a coefficient of 0.2–0.4 against steel). Design for shear, not pull-off, when the magnet is used to hold something vertically.
  • Temperature. Remanence falls roughly 0.11% per °C for standard NdFeB grades, so a magnet at 120 °C produces about 11% less flux and around 20% less force than at 20 °C, before any irreversible loss is considered.
  • Partial contact. If the magnet overhangs the steel edge or sits on a curved surface, only part of the pole face contributes, and the area term in the formula must be reduced accordingly.
  • Area mismatch. A magnet wider than the steel beneath it wastes flux at the edges; a magnet narrower than a saturated thin panel is limited by the panel, not by the magnet.
  • Corrosion and contamination. Rust, oil films and grit all behave as distributed air gaps and reduce force, sometimes by 10–30% over the life of an outdoor installation.
  • Safety factor. Always apply a margin — a factor of two or more for static holding, and higher for vibration, thermal cycling or personnel-safety duties.

“Can I trust a calculated pull force for a safety-critical magnet?” — No. Use the calculation to size the design, then verify the finished assembly with a pull test on production-representative steel, and keep a substantial margin for shear, temperature and ageing.

Decision Framework: Five Inputs That Fix the Answer

Work through these inputs in order. Each one narrows the result, and together they turn the formula into a usable design figure:

  1. What is the effective pole face area, and how many pole faces contact the steel? A pot magnet uses two; a plain disc uses one. This sets the A term directly.
  2. What is the interface flux density B at the intended gap? Start from the table above, then reduce it for the actual air gap and steel thickness, or measure it on a sample.
  3. How thick and what grade is the steel return path? Thin or non-magnetic steel caps the force regardless of magnet grade.
  4. How is the load applied — direct pull or shear? For shear, use the friction-limited figure, not the pull-off figure, and add a generous margin.
  5. What is the worst-case temperature and environment? Reduce B for temperature and add a factor for corrosion, contamination and fatigue over the service life.

Applied in sequence, these five inputs usually reveal that the binding constraint is the circuit and the gap rather than the magnet grade. A slightly stronger grade rarely rescues a design that has been given a 1 mm air gap or a thin steel backing, whereas closing the gap or thickening the steel often doubles the usable force at no material cost.

In short: estimate B at the interface, multiply the area by the magnetic pressure it produces, then subtract for air gap, steel thickness, load direction and temperature. The formula is simple; the engineering is in choosing B honestly for the assembly that will actually be built.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top