Skip to content
Welcome to ATM-Magnet
Application Notes

Magnet industry insights, product updates and application notes from ATM-Magnet.

Pot Magnets: Ultimate Guide to Mounting and Load Ratings

Published:2026-10-16    Category:Application Notes    Views:2

Pot magnets are holding assemblies made from a magnet enclosed in a steel cup, and the cup is the reason they outperform a bare magnet of the same size. The steel housing acts as the return path for flux and concentrates the magnetic field onto a single working face, so the assembly typically holds two to four times the load of an unmounted magnet. Because the housing also provides the mounting feature — a thread, a bore or a clamp — pot magnets are chosen as much for how they attach as for how strongly they grip.

The two decisions that determine performance are the mounting style and the load rating. Mounting style fixes how the assembly is fastened and in which direction the load can be applied; the load rating fixes how much it can safely hold. Both come with conditions that are frequently ignored, which is why a pot magnet that “should” hold 30 kg sometimes fails at 5 kg in service.

What Are Pot Magnets and How Do They Work?

A pot magnet consists of three parts: a magnet core, a steel cup that surrounds it on all but one face, and a mounting feature machined into or welded onto the cup. The open face is the working pole. Flux leaves that face, crosses the air gap into the target steel, and returns through the cup wall rather than through the surrounding air. The result is a short, low-reluctance circuit with almost all the useful field concentrated where it is wanted.

This geometry explains the two advantages that make pot magnets so common in fixtures, jigs and holding applications. First, the flux is confined to one face instead of being split between two, so the holding force per unit of magnet volume is much higher. Second, the housing shields the sides of the assembly, so a pot magnet can be placed close to sensors or adjacent hardware with far less interference than an exposed magnet would cause.

“What is the difference between a pot magnet and a plain magnet?” — The steel pot is a return path. It concentrates flux on one face, which is why pot magnets usually hold two to four times the load of a bare magnet of the same diameter.

Mounting Styles Compared: Threaded, Bore, Clamp and Flat-Bar

Mounting style is usually the first thing to fix, because it determines the geometry of the surrounding fixture. Threaded versions give a positive, adjustable connection; bore versions suit a through-bolt; clamp and bar types spread the holding force over a wider area. The table below covers the common industrial configurations.

Mounting Style How It Attaches Typical Body Sizes Load Direction Best For
Threaded stud (male) Bolt through a bracket or nut Ø16–Ø75 mm Normal to the face Fixtures, jigs, signage, signage boards
Threaded bore (female) Screw into the housing Ø20–Ø88 mm Normal to the face Sensors, clamps, adjustable stops
Plain bore / countersunk Through-bolt or countersunk screw Ø16–Ø63 mm Normal to the face Panels, handles, latches, flush mounting
Clamp / flat bar Clamped to a frame or track Bars 40–300 mm long Normal or in shear Wide-area holding, doors, tool holders
U-shape / channel Two pole faces in one body 40–200 mm bodies Across the gap Magnetic catches, grippers, door closures
Rubber-coated Bonded onto a coated base Ø22–Ø88 mm Normal to the face Protecting painted or finished surfaces

Which Housing Material and Magnet Core Should You Choose?

The housing and the core magnet are chosen together, because the operating temperature and the environment set the limits on both. A zinc-plated steel housing with a standard NdFeB core suits most indoor fixtures; a stainless housing with an SmCo core is the answer for marine, chemical or high-temperature duty. Note that a stainless housing is not itself magnetic — the holding force still comes from the core, and the thicker stainless wall slightly reduces the available pull.

Housing Corrosion Resistance Typical Service Temperature Notes
Zinc-plated steel Moderate up to 80 °C Standard and lowest cost
Nickel-plated steel Good up to 80 °C Better wear resistance and appearance
Stainless 304 housing, NdFeB core Very good up to 80 °C Outdoor and washdown; slightly lower pull
Stainless 316 housing, SmCo core Excellent 250–300 °C Marine, chemical and high-temperature duty
Rubber-coated steel Moderate up to 80 °C Protects finished surfaces; adds an air gap
Plastic or brass housing Good depends on core Light duty and decorative use
Core Magnet Typical Grades Max Operating Temperature Relative Holding Force Notes
Sintered NdFeB N35–N52 80 °C (N), 120 °C (H), 150 °C (SH) Highest (baseline 1.0) Default core for pot magnets
SmCo 2:17 series 250–350 °C 0.6–0.8 High temperature and good corrosion resistance
Ferrite (ceramic) Y30–Y35 250 °C 0.25–0.35 Low cost, high temperature, low force
Bonded NdFeB BN series 100–120 °C 0.4–0.6 Complex shapes, lower force

How Are Load Ratings Determined and How Do You De-Rate Them?

A published load rating for pot magnets is a laboratory figure. It is measured on a polished, flat, thick mild-steel plate with full contact, at room temperature, with the load applied perpendicular to the working face and pulled directly away. Every one of those conditions is generous compared with real service, which is why the catalogue number should be treated as a starting point rather than a working limit.

The practical rule is to apply a safety factor of at least three to one, and five to one or more where vibration, shock or overhead use is involved. The factor is applied to the actual load, not to the rated pull, and the de-rated capacity must still exceed the load after all the penalising conditions in the table below have been accounted for.

De-Rating Factor Typical Effect on Rated Pull Reason Mitigation
Air gap (0.2 mm paint layer) 40–60% retained Reluctance rises steeply with gap Contact bare steel; strip coating at the face
Rough or non-flat surface 30–70% retained Partial contact and local gaps Machine, grind or face the target surface
Thin target sheet 50–80% retained Return path saturates in thin material Increase sheet thickness above the magnet diameter
Temperature rise 5–20% loss toward 80 °C Reversible loss, then irreversible loss Use H or SH grade, or an SmCo core
Load applied in shear 10–30% of the normal pull Shear capacity depends mainly on friction Add a mechanical stop or change the load direction
Oil, dust or mill scale 10–40% loss Contaminant holds the magnet off the surface Clean the contact faces before use
Non-ferrous target (304, aluminium) close to zero No flux return path exists Provide a ferromagnetic counterface

“Why does my pot magnet hold less than the catalogue figure?” — Air gap is the usual answer. Paint, galvanising, scale or a rough surface adds a gap in series with the working air gap, and pull force falls away quickly as that gap grows.

Worked Example: Sizing Pot Magnets for a Vertical Lift

Suppose an assembly weighing 5 kg is held against a painted steel column and the load acts perpendicular to the magnet face. The calculation below shows how the rated pull, the safety factor and the de-rating conditions combine.

Step What to Calculate Example Result
1. Actual load m × g = 5 × 9.81 49 N
2. Minimum rated pull at 4:1 safety factor 49 × 4 ≥ 196 N
3. Catalogue selection Ø32 mm pot magnet, polished steel rating 330 N
4. Air gap de-rating (0.2 mm paint) 330 × 0.6 198 N
5. Temperature de-rating (60 °C) 198 × 0.9 178 N
6. Margin check 178 N available vs 49 N load 3.6 × margin — acceptable

Two lessons follow from the numbers. First, the de-rating step matters more than the initial selection: a magnet chosen only against the 49 N load would have been much smaller than the correct one. Second, if the same load had acted in shear rather than perpendicular to the face, the available capacity would have dropped to roughly 30–60 N and the design would have needed either a larger assembly or a mechanical stop.

“Can pot magnets be used for overhead lifting?” — Only with a generous safety factor and a firm understanding of how much the real conditions de-rate the rating. They are not certified lifting devices. Quoted pull assumes polished steel, full contact and perpendicular loading — rarely the situation in service.

Decision Framework: Six Inputs for Selecting Pot Magnets

  1. How will the assembly attach? Threaded, bore, clamp or U-shape — this follows from the surrounding fixture, not from the magnet.
  2. What is the direction of the load? Perpendicular to the face uses the full rating; shear uses only a fraction of it.
  3. How good is the contact surface? Painted, galvanised or rough steel adds an air gap and throws away a large part of the rating.
  4. What is the working temperature? It fixes the core grade: N, H or SH-grade NdFeB, or SmCo for the hottest duty.
  5. What environment will it see? Outdoor, marine or washdown duty calls for a stainless housing rather than zinc plating.
  6. What safety factor does the application demand? Three to one for static indoor holding, five to one or more where vibration, shock or height is involved.

Worked in this order, these six inputs turn a catalogue number into a defensible holding capacity — and they are the reason two engineers can specify the same size of pot magnet and end up with very different real-world results.

To summarize: a pot magnet is a magnet plus a steel return path, which is why the housing concentrates flux on one face and roughly doubles to quadruples the holding force. Mounting style decides how the assembly attaches and in which direction it can be loaded; housing material and core grade decide the environment and temperature it survives; and the load rating is only valid under ideal laboratory conditions, so it must always be de-rated for air gap, surface finish, target thickness, temperature and load direction, and then checked against a safety factor. Pot magnets are simple assemblies, but the numbers behind them need the same discipline as any other magnetic design.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top