Magnet density is the cheapest quality signal in the entire permanent-magnet supply chain, and the one most buyers never look at. A sintered NdFeB part that weighs light is not saving you freight — it is telling you that porosity, under-sintering or contamination has taken up residence inside the magnetic circuit you are paying for. The number is one balance weighing away, and it quietly validates or invalidates half the claims on a material certificate. These five checks turn magnet density from a forgotten line item into a routine acceptance tool.

Check 1: Measure Magnet Density by Archimedes, Not by Trust

The hydrostatic weighing method is five minutes of work and needs no certificate. Weigh the dry part in air, suspend it from a fine wire in deionised water, weigh again, and density equals the air weight divided by the loss of weight, multiplied by water density corrected to the lab temperature. For a machined part with through-holes, that number is the true solid fraction of the material, not of the geometry — the method counts only the volume the metal occupies.

Two habits keep the number honest: wet the part fully before the immersed weighing, because trapped air bubbles read as porosity that does not exist, and dry the surface completely before the air weighing, because a water film reads as extra density. Run three parts per lot and take the spread, not just the mean — porosity is a scatter phenomenon.

Check 2: Compare Against the Grade’s Theoretical Density

A measured number means nothing without the right reference. Sintered NdFeB theoretical density runs roughly 7.4–7.6 g/cm³ depending on composition — heavy-rare-earth-rich grades sit higher, cerium-bearing formulations slightly lower. A healthy sintered lot lands at 98.5–99.5 percent of its own theoretical value, and anything below 98 percent deserves a question before the parts go into a magnetic circuit.

The comparison must be grade-aware, because the common buyer error is judging all NdFeB against one number and calling a legitimate 7.42 g/cm³ Dy-rich part “dense” while calling a 7.55 heavy-grade part “light.” Ask the supplier for the theoretical density of the specific alloy formulation, and measure magnet density against that figure — the same way the mill does.

Check 3: Read the Porosity in the Fracture Surface

Density tells you how much porosity; the fracture tells you what kind. Snap a sacrificial piece and look at the broken surface under a low-power loupe. Fine, evenly distributed micro-voids with a metallic sheen between them are normal sintering residue and mostly harmless. Large irregular cavities, dark films, or a surface that looks like frozen foam point to real problems — under-sintering, too-fast heating with binder burn-out damage, or oxide contamination — and the difference matters because pore shape decides whether the voids are merely diluting the magnet or actively cracking it.

Open, interconnected porosity is the worst signature of all: it is the corrosion pathway that turns the inter-granular attack mechanism into an inside-out failure, and it drinks coating solutions instead of accepting them.

Check 4: Trace the Cause — Press, Sinter Curve, Furnace Load

Porosity has a short list of parents, and a supplier who knows density drift can usually name which one moved. Green density too low: the die press pressure or powder fill volume slipped, leaving more shrinkage to close than the sinter can achieve. Sinter temperature or time short: the liquid-phase densification never finished its work — the classic under-fired lot. Heating ramp too fast: binder gases blow channels through the compact. Crucible or furnace-load contamination: excess oxygen and carbon stabilise pores at grain boundaries. Overloaded setters: parts touching each other, or sitting in a cold corner of the chamber, densify unevenly inside one load — which is exactly why the three-part scatter from Check 1 is the statistic to watch.

Check 5: Convert Density Loss into Magnetic Loss

This is the check that makes the number commercial. Pores are non-magnetic volume. A lot at 97 percent of theoretical density carries roughly three percent less magnetic material per part than a lot at 100 percent, and remanence and total flux scale with that missing volume almost one-for-one: Br, pull force at a fixed gap, and energy product all read light. The corollary is uncomfortable but useful — a magnet whose Br sits below certificate spec while its magnet density reads low is not suffering a measurement dispute; it is suffering the same voids twice.

Strength is the second victim, and the more dangerous one: pores and especially micro-cracks around them cut flexural strength disproportionately, and NdFeB is already a brittle ceramic-like material. A 2 percent density loss can carry a 10 percent or more strength loss, which shows up as chipped corners in grinding and shattered parts at assembly snap.

When 98 Percent Is Fine and When It Is Not

Context decides the acceptance line. A dense, well-sintered part at 98.5 percent in a sensor assembly that never sees mechanical abuse is genuinely fine — the residual closed microporosity costs a fraction of a percent of flux and nothing else. The same 98.5 percent in a large ring magnet that will be press-fitted, or a part destined for humid service where open porosity can wick moisture, is a different conversation. And for bonded magnets the entire frame changes: resin-bonded parts run 6.0–6.7 g/cm³ by design, and judging them against sintered references is simply the wrong test.

Material Theoretical Density (g/cm³) Typical As-Manufactured Density Solid Fraction Comment
Sintered NdFeB 7.4–7.6 7.3–7.5 (98.5–99.5%) Below 98% — question the sinter
Bonded NdFeB 6.0–6.7 As-formulated Resin is designed in, not porosity
SmCo 8.2–8.4 8.1–8.3 Same sintering logic, higher baseline
Alnico (cast) 7.3–7.5 Cast — near-fully dense Shrinkage cavities, not sinter porosity
Hard ferrite (ceramic) 4.8–5.0 4.5–4.8 (90–96%) Higher residual porosity is normal

Q: Can a gaussmeter or flux reading replace the density check?
A: They answer different questions and the two cross-check each other. A flux reading tells you the magnetic circuit is short; it does not tell you whether voids, poor alignment or a measurement error caused it. Density does the opposite. When flux is low and density is normal, look at the magnetisation and the test setup; when both are low, the sinter is the suspect.

Q: Does a light magnet always mean a bad magnet?
A: No — verify the reference before the verdict. Coatings, oil film, a wire loop left on the part during weighing, or simply the wrong theoretical density for the alloy all produce false alarms. A genuine 1–2 percent shortfall against the correct grade reference is real, and worth a fracture look under Check 3.

Is Your Magnet Density Report Complete?

Four questions to put to any certificate or incoming inspection.

1. Does the report state the measured value, the theoretical reference, and the method? A bare number without the grade-specific reference and the weighing conditions is decoration. Archimedes, three parts, lot scatter — that is a report.

2. Is the acceptance line tied to your application? 98 percent may pass a datasheet and fail your press-fit. Set the line where Check 5’s flux math and Check 3’s fracture evidence say your part needs it.

3. Does the supplier keep the fracture record, not just the weight? Ask for the loupe picture from sacrificial pieces per lot. Density drift with pore morphology attached is a process story; density alone is a weather report.

4. Do magnet density and Br move together in your incoming data? Correlated lows confirm porosity is stealing flux; uncorrelated lows mean something else — alignment, magnetising fixture, measurement — and your next corrective action is in a different department.

To Summary

  • Archimedes weighing takes minutes, needs three parts per lot, and validates half the certificate.
  • Compare against the specific alloy’s theoretical density — grade-aware or the number lies.
  • The fracture shows what the balance cannot: pore shape, distribution and the open-porosity corrosion risk.
  • Every percent of density loss costs roughly a percent of flux and a disproportionate share of strength.
  • Make magnet density a standing incoming check: it is the cheapest process alarm you can buy.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top