The Three Families Behind Magnet Coatings
Zinc is electroplated soft and grey, deliberately anodic to the NdFeB substrate: at any scratch or pore it corrodes itself instead of letting the magnet corrode, and its white corrosion products stay permeable enough that the film keeps working as it consumes. Tin is a true barrier — slightly noble to the substrate, chemically gentle, exceptionally solderable, and the standard answer when a magnet must later be soldered or brazed into an assembly. Chrome is the hard one: micro-cracked electroplated chromium delivering 700–1000 HV of wear resistance and a mirror look, used where abrasion, not humidity, is the enemy.
| Attribute | Zinc | Tin | Chrome |
|---|---|---|---|
| Galvanic role vs NdFeB | Anodic — sacrificial | Cathodic — barrier | Cathodic — barrier |
| Typical thickness | 5–15 µm | 5–12 µm | 10–25 µm over nickel base |
| Neutral salt spray to first red oxide | 24–96 h | 12–48 h | 24–72 h |
| Mechanical character | Soft, tolerates impact | Soft, low friction | Very hard, brittle |
| Signature niche | Humid service with handling damage | Soldering, brazing, food-contact proximity | Wear faces, chucks, sliding contact |
| Main failure mode | Consumed fast in alkali or acid | Pitting at any pore once breached | Cracking at magnet impact points |
| Relative cost | Low | Medium | High |
Read the table as three different bets about how the coating will be damaged, because magnet coatings are chosen by failure mode, not by preference.
Trade-off 1: Sacrificial Protection vs Barrier Protection
Zinc bets that the part will be scratched; tin and chrome bet that it will not. A chipped zinc film keeps protecting the exposed magnet because the surrounding zinc corrodes preferentially and its products blanket the defect. A pore in tin or chrome does the opposite — the whole coating area becomes a cathode feeding a tiny anodic pit, the same galvanic trap that makes NiCuNi plating thickness-sensitive. If your assembly process involves magnets snapping together by hand, the sacrificial bet is the honest one.
Trade-off 2: Ductility vs Wear Resistance
You cannot have both in one electroplated metal. Zinc and tin are soft enough to yield with the substrate and shrug off impact chipping, but they polish away under sliding contact within months. Chrome reverses the profile: it will outlast every other finish on a magnetic chuck face that parts slide across all day, but a single hard magnet-to-magnet impact can crack it through to the base metal, and the crack then behaves like a defect of the barrier family. Specify by the dominant damage mechanism — impact or abrasion — not by how the coating looks on arrival.
Trade-off 3: Solderability vs Salt-Spray Life
Tin is the only common magnet finish a downstream process can wet solder onto, which is why sensor and loudspeaker assemblies that are reflowed or hand-soldered specify it even though its salt-spray envelope is the shortest of the three. That is a deliberate trade: the assembly step is guaranteed, the environment is assumed benign. Putting tin on an outdoor bracket, or zinc where a solder joint is planned, is the classic specification error in this family.
Trade-off 4: Appearance vs Survivability
Chrome wins the shelf-appeal argument outright — mirror brightness, no colour drift, the finish buyers associate with quality. Zinc is matte grey and blooms white; tin is satin and dulls. But appearance-driven specification hides a survivability cost: chrome’s brightness is deposited over a nickel base, adding process steps, cost and a second galvanic interface, all to protect a part that will be invisible inside its housing anyway. If the magnet disappears into an assembly at minute one of service, buy the finish that survives, not the one that photographs.
Trade-off 5: Cost vs Verified Performance
Per part, zinc is the cheapest of the three, tin sits mid-range with metal-price volatility, and chrome costs most because it is effectively two coatings. But unit price is the wrong denominator when the failure mode is a stopped line. The right comparison is cost per verified service envelope: a zinc film with a reported 96-hour salt-spray result on your geometry usually beats a chrome film with no data at the same price, and both beat an untested bargain finish that becomes a warranty event.
Q: Can zinc, tin or chrome replace NiCuNi entirely?
A: They replace it by role, not by rank. Zinc wins where impact chipping is certain; tin wins where soldering is required; chrome wins where abrasion dominates. For balanced indoor-to-weathered service with a bright finish, the nickel stack remains the general-purpose default.Q: Are white deposits on my zinc-plated magnets a failure?
A: No — that is zinc working as designed. White corrosion product is sacrificial action at the surface. Red-brown bloom underneath it is the real warning: the zinc has been consumed at that spot and the magnet is now exposed.
Which of These Magnet Coatings Fits Your Part?
Four questions close the gap between the table and your drawing.
1. What damages the part first — impact, abrasion, humidity or process heat? Impact points to zinc, abrasion to chrome, humidity with no damage to a nickel barrier, downstream soldering to tin. Name the enemy before naming the metal.
2. Is the defect population zero or assumed? If any pore or scratch is likely in production or assembly, cathodic barrier finishes inherit the pitting trap; sacrificial finishes forgive it.
3. Will the finish be seen by a paying customer? If yes, chrome or nickel earns its cost. If the part is buried, redirect that budget to thickness and test data.
4. Does the supplier report salt-spray hours on your geometry? Generic datasheet numbers describe flat panels, not chamfered ring magnets with thin edges. Magnet coatings earn their specification on verified, part-shaped evidence.
To Summary
- Zinc is sacrificial: it protects defects by consuming itself, tolerates impact, and fails fastest in alkali and acid.
- Tin is a solderable barrier with the shortest salt-spray envelope — chosen for assembly processes, not for weather.
- Chrome is the wear and appearance champion, brittle under magnet impact and priced as a two-coating system.
- Choose by dominant damage mechanism, then by defect population, visibility and verified test data.
- Cost per verified service envelope — not unit price — is the honest comparison across magnet coatings.