Y30, Y35 and Y40 Ferrite Grades: What the Numbers Mean

Order ferrite grades by their numbers and you will eventually get burned: two parts both labeled Y35, one holding a field the other lost in a week, or a “better” Y40 that demagnetizes where a Y30 survived. The confusion is not your fault — the numbering system is a shorthand invented for factory floor talk, not for design engineers. The good news is that a handful of rules decode it completely. Once you know what the digits measure, what the suffixes add, and what the datasheet quietly leaves out, ferrite grades stop being lottery tickets and become predictable engineering inputs.

Rule 1: The Number Is Energy Product — and Nothing Else

The Y-series digits used across Chinese ceramic magnet factories — Y30, Y32, Y33, Y35, Y38, Y40 — encode exactly one property: nominal maximum energy product, (BH)max, in units of MGOe multiplied by ten. Y30 means roughly 3.0 MGOe (about 230–240 kJ/m³), Y35 means about 3.5 MGOe, and Y40 means about 4.0 MGOe. That is the entire secret of the naming. The number says nothing about coercivity, nothing about temperature behavior, and nothing about remanence beyond the weak correlation that higher grades do push Br from roughly 0.39 T up to 0.42–0.43 T. Designers who read “Y40 is stronger than Y30” as a blanket statement are reading meaning into digits that was never there.

Parameter Y30 Y35 Y40
Nominal (BH)max 2.7 – 3.1 MGOe 3.3 – 3.7 MGOe 3.8 – 4.2 MGOe
Remanence Br 0.38 – 0.40 T 0.40 – 0.41 T 0.41 – 0.43 T
Normal coercivity Hcb 240 – 260 kA/m 250 – 270 kA/m 280 – 300 kA/m
Intrinsic coercivity Hcj 3.0 – 3.6 kOe 3.2 – 3.6 kOe 3.5 – 4.0 kOe
Density 4.5 – 4.7 g/cm³ 4.7 – 4.9 g/cm³ 4.8 – 5.0 g/cm³

Rule 2: Within Ferrite Grades, Coercivity Trades Against Energy

Pushing (BH)max higher means denser pressing, finer powder, and better crystal alignment — and every one of those levers nudges the microstructure toward larger grains, which lowers coercivity in the standard variant of a grade. Across the Y-series the energy-product gain from Y30 to Y40 is real but modest, while the practical spread in demagnetization resistance comes from how each grade was formulated and pressed. The consequence for design: a Y40 chosen blindly is not automatically more robust than a Y30 in a reversed-field duty. Compare the Hcj line on the datasheet, never the headline number alone — it is the single most common mistake in specifying ferrite grades.

“Is Y40 always better than Y30?” — Only in energy product per volume. If your circuit is closed and space is tight, Y40 wins. If the magnet faces shock fields or thin iron paths, a high-coercivity Y30Y can outperform Y40 in the field despite its lower headline grade.

Rule 3: The Suffix Changes the Magnet More Than the Number

A trailing “Y” — Y30Y, Y35Y — flags the high-coercivity variant of that grade, achieved by cobalt-substituting the hexaferrite crystal. The Y-suffix versions typically add 15–30% to intrinsic coercivity while giving back a little remanence. For engineers, this suffix is the most important word on the purchase order: Y30Y is the grade for motors with armature reaction, couplings with opposing rotors, and anything that sees fields trying to push it backward. Conversely, the same base number can also split into isotropic (Y30-1, multi-pole pressable, weaker) and anisotropic (die-pressed in a field, strongest along the press direction) families — another distinction the bare number hides completely.

Rule 4: How Ferrite Grades Are Made Decides Whether You Get Them

Ferrite grades are promises made by pressing. Isotropic parts are pressed in a die without a field — every grain points randomly, the magnet pulls equally from any face, and the real output lands well below the anisotropic rating of the same number. Anisotropic parts are wet- or dry-pressed inside a strong aligning field so the platelet crystals rotate into line; the grade number then holds along one axis only, and anything perpendicular is much weaker. A “Y35” ring magnetized through a multipole tool is therefore a different beast from a Y35 block pressed lengthwise. When you spec ferrite grades, state the press type, the magnetization direction, and the tolerance on each property — the number by itself guarantees none of them.

Rule 5: Price Tracks the Number; Cost per Joule Does Not

Each step up the Y-series costs money in finer powder, longer milling, better presses, and higher scrap — Y40 can quote 30–60% above Y30 per part. But the energy gain is only about 30%, and the density gain means more material per joule too. Run the cost-per-joule arithmetic and the “premium” grade is often the worse buy unless your constraint is volume: Y40 earns its surcharge exactly when the housing cannot grow. If space is free and the circuit is closed, Y30 or Y32 delivers the same flux for less — one more reason the biggest number is not automatically the best grade.

Which Grade Is Right? Answer These 4 Questions

  • Is the magnetic circuit closed with generous iron, or semi-open with reverse fields? Reverse fields point to the Y-suffix high-coercivity variants before they point to a bigger number.
  • How much volume can the housing spare? If space is not binding, Y30/Y32 cost-per-joule beats Y40 every time.
  • Does the part magnetize along the press axis? Anisotropic grades only pay out along their alignment direction; multi-pole or isotropic duty changes the grade you actually need.
  • Are you buying a number or a curve? Demand Hcb, Hcj, Br and density with limits on the datasheet — the grade label is a nickname, not a specification.

To Summary

The digits in ferrite grades measure one thing — energy product times ten — and leave out everything else that decides whether a magnet survives your application. Coercivity lives in the suffix, directionality lives in the press method, and value lives in the cost-per-joule arithmetic, not in the headline number. Read the full curve, not the nickname: match Y30, Y35 or Y40 to your circuit’s real demagnetizing stress and available volume, and the right grade is usually the cheaper one than you assumed.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top